轧制压下率、路径对NiCoCr合金微观结构和力学性能的影响

The effects of cold rolling thickness reduction and path on the microstructure and mechanical properties of NiCoCr alloy

  • 摘要: 通过开展不同轧制压下率和路径的轧制实验,制备了具有不同比例和尺寸的纳米孪晶和纳米晶结构 NiCoCr 合金。透射电镜表征结果表明,单向轧制压下率50%样品中微观结构特征以纳米孪晶和高密度位错为主。当压下率达到90%,由于剪切带在纳米孪晶片层结构中的开动,孪晶体积分数下降,同时剪切带内形成大量尺寸为35 nm的纳米晶结构。多方向轧制样品中微观结构以纳米晶结构为主,平均尺寸为27 nm,略小于单向轧制压下率90%样品中的纳米晶尺寸。拉伸实验结果表明:相比于轧制前固溶态粗晶合金,单向轧制压下率50%纳米孪晶镍基合金强度大幅提高,合金屈服强度和抗拉强度分别达到1 312 MPa和1 396 MPa。压下率90%轧制样品屈服强度高达1 599 MPa,变方向轧制样品屈服强度更是高达1 705 MPa。同时拉伸试验数据表明,晶粒细化可以有效地提高材料强度,但是材料的延伸率显著下降。

     

    Abstract: Bulk NiCoCr alloy samples with different volume fraction of nano-twins and nano-grains were fabricated by cold rolling with various thickness reduction and strain path. Transmission electron microscopy observations indicate that the microstructure in the one-directional rolled sample with 50% thickness reduction is characterized by nano-twins and high density of dislocations. With increasing the rolling thickness reduction to 90%, the volume fraction of nano-twins decreases due to the activation of shear banding within the nano-twined lamellar area, which consequently leads to the formation of massive nano-grains with average sizes of 35 nm. The microstructure of the multi-directional rolled sample is mainly composed of nano-grains with main sizes of 27 nm, which is slightly smaller than that of one-directional rolled sample. Tensile test results show that the strength of the one-directional rolled sample with 50% thickness reduction is significantly enhanced with yield strength and ultimate tensile strength reaching 1 312 MPa and 1 396 MPa, respectively, which is much higher as compared to the coarse-grained alloy with solid solution heat treatment. The yield strength is further increased to 1 599 MPa with thickness reduction reaching 90%, and multiple-directional rolling gives rise to a higher yield strength of 1 705 MPa. Tensile testing results indicated that the grain refinement could significantly increase the strength, but deteriorate the ductility to some extent.

     

/