Ti9148钛合金β-相晶粒长大行为

Grain growth behavior in the β- phase of Ti9148 titanium alloy

  • 摘要: Ti9148合金为一种新研制的生物医用钛合金。为了合理控制生产过程中产品的晶粒尺寸,文中通过固溶淬火实验研究了Ti9148钛合金β-相晶粒在不同加热温度和保温时间固溶处理时的长大行为。结果表明:随着加热温度的升高,Ti9148钛合金β-相晶粒尺寸不断增大,并且温度越高,增长速度越快;在等温加热过程中,随着时间的延长,β-相晶粒尺寸先快速长大,超过30 min后,增速减缓。晶粒长大动力学表明:Ti9148钛合金在750~900 ℃等温加热时,β-相晶粒尺寸与保温时间近似成幂函数关系,晶粒生长指数约为0.213~0.300;计算得到Ti9148钛合金β-相晶粒的长大激活能为32.57 kJ/mol。

     

    Abstract: Ti9148 alloy is a new biomedical titanium alloy. To reasonably control the grain size of the product in the production process, the β-grain growth behavior of Ti9148 titanium alloy at different solution treatment temperatures and holding times was studied by solution quenching experiments. The results showed that the β-grain size of the alloy increased with increasing heating temperature, and the higher the temperature was, the faster the grain size grew. In the isothermal heating process, the β-grain size first grew rapidly and then slowed down after more than 30 min. The grain growth kinetics showed that when the alloy was heated at 750-900 ℃, the relationship between the β-grain size and holding time approximated a power function, and the grain growth index was approximately 0.213-0.300. The activation energy of grain growth was calculated to be 32.57 kJ/mol.

     

/