ZHONG Sheng-wen, WANG Yu-xiang, ZHANG Qian, WEN Xiao-qiang. The discoloration pearl platelets preparation by molten salt method[J]. Nonferrous Metals Science and Engineering, 2013, 4(2): 79-84. DOI: 10.13264/j.cnki.ysjskx.2013.02.005
Citation: ZHONG Sheng-wen, WANG Yu-xiang, ZHANG Qian, WEN Xiao-qiang. The discoloration pearl platelets preparation by molten salt method[J]. Nonferrous Metals Science and Engineering, 2013, 4(2): 79-84. DOI: 10.13264/j.cnki.ysjskx.2013.02.005

The discoloration pearl platelets preparation by molten salt method

  • neodymium color powder was synthesized by molten salt method with the neodymium chloride (NdCl3·6H2O) and caustic soda (NaOH) as raw materials, using sulfate as flux respectively. The influence factors on the morphology and crystal form, including the type and amount of molten salt, sintering conditions and additives incorporation were investigated. The color powder was characterized by optical microscope, SEM, XRD, and ICP. The results show that, neodymium color powder can be prepared by molten salt method at 900~1 200 ℃ for three hours using Na2SO4-K2SO4 as flux respectively. The molar ration of molten salt and color powder is 4:1 with good pearlescent and discoloration effects.
  • loading

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return